Integrity issue
A 14 inch section of duplex pipework containing gas had mechanical cracking at one of the welds. An engineered Futurewrap repair was sought to both strengthen the pipework as well as prevent the external atmosphere attacking the weld. To reinstate the integrity of this section of this 14 inch line, it was proposed to use a Futurewrap Glass/HT composite repair.
Design
The design of the Futurewrap Glass/HT repair was to strengthen the pipework. The design parameters were; pressure 10 bar, temperature 1450C, design lifetime 10 years. It was assumed that the composite repair would withstand the applied load without any allowance for remaining steel. The design resulted in a thickness of 7 mm (9 layers) of
Futurewrap Glass/HT composite repair with an axial length of 300 mm.
Installation
The installation steps are shown in the photographs. The repair was applied off ropes as the pipework is elevated. The surface preparation was to ST3. Full QA/QC measurements were made to demonstrate that the Futurewrap repair was applied in accordance with ISO 24817.
Summary
A 14 inch diameter production line suffering mechanical cracking at a weld was repaired using Futurewrap Glass/HT composite repair. The repair was completed within 3 days reinstating the integrity of the pipework.